T6 Temper 7075 Aircraft Grade Aluminum Thin Sheet Stress Corrosion Cracking Resistant

JIMA Aluminum
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

T6 Temper 7075 Aircraft Grade Aluminum Thin Sheet Stress Corrosion Cracking Resistant

Brand Name : JIMA Aluminum

Model Number : 7075

Certification : IRIS,ISO9001,ISO 14001, IRIS.

Place of Origin : CHINA

MOQ : Negotiations

Price : Negotiations

Payment Terms : T/T, L/C

Supply Ability : 1000 MT/ per month

Delivery Time : 20~30days

Packaging Details : wooden pallet

application : automobile

shape : plate,sheet,panel

Standard : EN485-2008

name : Aluminum thin sheet 7075 T6

alloy : 7075

Temper : t6

Contact Now

Products Name:

Aluminum thin sheet 7075 T6 dimension 0.2mm 0.4mm 0.5mm for aerospace applications

Features of Aluminum sheet 7075 T6

  • 7075 aluminum sheet is among the highest strength alloys available and used in highly stressed parts.
  • Corrosion resistance and machinability are rated as fair,
  • Though the addition of chromium provides good stress-corrosion cracking resistance in 7075 aluminum sheet products

Application of Aluminum sheet 7075 T6

  • Aerospace applications

7075 aluminum thick plate sizes:

7075 t6 T:0.2~3*1250*2500mm,0.2~3*1500*3000mm

Chemical Composition Limits (WT%):

Alloy Si Fe Cu Mn Mg Cr Zn Ti Others
each total
7075 0.4 0.5 1.20-2.00 0.3 2.1-2.9 0.18-2.8 5.10-6.10 0.2 0.05 0.15

7075 t6 Aluminum Plate Typical Mechanical Properties:

Temper Tensile Strength Yield Strength Elongation
KSI KSI %
O (annealed) 40 21 9-10
T6 74-78 63-69 5-8
T651 75-67 66-54 9-3

Packaging Details

Packaging Details 1 tons
Produce Capacity 2500 tons/Month
Sample Making About one week after we get the charges
Payment Item T/T,30% prepayment,balance before shipment. Irrevocable L/C at sight
Delivery Time 30-60 days after receiving the prepayment

Packaging Details

Standard export package.

One pallet is about 2-3 ton.Two steel belts in width and three in width.

One 20GP container can load about 18-20 tons aluminum sheet.

One 40GP container can load about 24 tons aluminum sheet

FAQ:

Q: Can you provide samples?
A: Yes ,can be suppliy

Q: How to contact your company?
A: With Skype or Email or the other ways we have written upon.

Q: Can you do customized design and size?
A:Yes, can be
customized as request.


Q: How to ensure the quality?
A:We have QC Team(Quality Certification),theMTC,SGS Certificate and MIDS can be supply
B:SGS inspection is okay.

7075 Aluminum Thick Plate Photos:

T6 Temper 7075 Aircraft Grade Aluminum Thin Sheet Stress Corrosion Cracking Resistant


Product Tags:

7075 aircraft grade aluminum

      

7075 aluminum plate

      
Best T6 Temper 7075 Aircraft Grade Aluminum Thin Sheet Stress Corrosion Cracking Resistant wholesale

T6 Temper 7075 Aircraft Grade Aluminum Thin Sheet Stress Corrosion Cracking Resistant Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: JIMA Aluminum
*Subject:
*Message:
Characters Remaining: (0/3000)